The main raw materials of IK-902 non curing rubber asphalt waterproof coating are a variety of high molecular polymers and special additives. The additive acts as a special catalyst to form a stable chemical combination between asphalt and various high molecular polymers. The waterproof coating can adopt various construction methods such as coating, spraying and grouting to stop leakage. At the same time, it can also be combined with various coiled materials. It is an international leading new waterproof material.
No. |
Item |
Index |
|
1 |
Flash point / ℃≥ |
180 |
|
2 |
Solid content /% ≥ |
98 |
|
3 |
Extensibility / mm ≥ |
15 |
|
4 |
Bonding properties |
Dry base |
100% cohesive failure |
5 |
Wet base |
||
6 |
Low temperature flexibility |
-20 ℃, no fracture |
|
7 |
Heat resistance / ℃ |
No sliding, flowing and dripping at 65 ℃ |